Properties of the PCR condition, compared with the other HDPE grades.

Recycled bottle/crate regrind for non-critical mouldings, pipes and lumber; property spread is wide and colour is limited to dark shades.

What is HDPE-PCR?

HDPE-PCR is HDPE in the PCR grade — recycled bottle/crate regrind for non-critical mouldings, pipes and lumber; property spread is wide and colour is limited to dark shades. HDPE-PCR has a yield strength of 22 MPa (3.19 ksi) and a tensile strength of 23 MPa (3.34 ksi) — weaker than 83% of polymer grades. Elongation at break is 200% and the elastic modulus is 1.1 GPa (0.16 Msi). HDPE-PCR has a density of 0.96 g/cm³ (0.0345 lb/in³), lighter than 74% of polymer grades. Its glass-transition temperature is -110°C (-166 °F). FDA Compliant is the default condition FabDigit quotes; PCR is available on request or by drawing note.

Advantages

  • Low embodied carbon — 0.7 kg CO₂/kg, better than 100% of polymer grades
  • Readily welded — 95/100, better than 99% of polymer grades
  • Conducts heat well — 0.48 W/m·K (0.277 BTU/hr·ft·°F), better than 97% of polymer grades
  • Low moisture uptake — 0.01%, better than 97% of polymer grades
  • Good corrosion resistance — 90/100, better than 81% of polymer grades

Limitations

  • Low strength — 22 MPa (3.19 ksi), worse than 83% of polymer grades
  • High mold shrinkage — 2%, worse than 81% of polymer grades
  • Hard to polish — 30/100, worse than 80% of polymer grades
  • Degrades in UV without stabilisers — 25/100, worse than 76% of polymer grades

HDPE-PCR properties

Typical room-temperature values for HDPE-PCR — 10 properties are specific to this condition; the rest are grade-level values shared by every HDPE grade. Each bar shows where the value sits among the polymer grades in FabDigit's library — further right is higher.

Physical6

HDPE-PCR has a density of 0.96 g/cm³ (0.0345 lb/in³), lighter than 74% of polymer grades. Its glass-transition temperature is -110°C (-166 °F).

Density0.96 g/cm³0.03 lb/in³
Melting Temperature (Tm)132°C270 °F
Glass Transition (Tg)-110°C-166 °F
Water Absorption (24 h)0.01%
Water Absorption (Saturation)0.05%
Refractive Index1.54

Mechanical16

HDPE-PCR has a yield strength of 22 MPa (3.19 ksi) and a tensile strength of 23 MPa (3.34 ksi) — weaker than 83% of polymer grades. Elongation at break is 200% and the elastic modulus is 1.1 GPa (0.16 Msi).

Elastic (Young's) Modulus1.1 GPa0.16 Msi
Shear Modulus0.4 GPa0.06 Msi
Bulk Modulus3 GPa0.44 Msi
Poisson's Ratio0.44
Tensile Strength (Ultimate)23 MPa3.3 ksi
Yield Strength (0.2% offset)22 MPa3.2 ksi
Elongation at Break200%
Compressive Strength22 MPa3.2 ksi
Compressive Modulus0.9 GPa0.13 Msi
Flexural Strength27 MPa3.9 ksi
Flexural Modulus1.2 GPa0.17 Msi
Shear Strength20 MPa2.9 ksi
Fracture Toughness (K_IC)2 MPa·√m1.8 ksi·√in
Izod Impact, Notched45 J/m0.84 ft·lbf/in
Hardness, Shore D65 Shore D
Hardness, Rockwell R55 HRR

Thermal11

HDPE-PCR is rated for continuous service to 80°C (176 °F). It conducts heat at 0.48 W/m·K (0.277 BTU/hr·ft·°F), better than 97% of polymer grades. Thermal expansion is 150 µm/m·K (83.3 µin/in·°F).

Thermal Conductivity0.48 W/m·K0.28 BTU/hr·ft·°F
Specific Heat Capacity1,900 J/kg·K0.45 BTU/lb·°F
Thermal Expansion (CTE, 20–100 °C)150 µm/m·K83.3 µin/in·°F
Max Service Temperature (continuous)80°C176 °F
Min Service Temperature-80°C-112 °F
Heat Deflection Temp. @ 0.45 MPa76°C169 °F
Heat Deflection Temp. @ 1.8 MPa47°C117 °F
Vicat Softening Point (B50)76°C169 °F
Flammability (UL 94)HB (burns slowly, drips); no self-extinguishing rating without FR package
Limiting Oxygen Index18%
Max Service Temperature (short-term)110°C230 °F

Electrical7

HDPE-PCR is an electrical insulator with a dielectric strength of 24 kV/mm (609.6 V/mil) and a resistivity of 1×10¹⁴ Ω·m.

Electrical Resistivity1×10¹⁴ Ω·m3.94×10²¹ µΩ·in
Dielectric Strength24 kV/mm610 V/mil
Dielectric Constant (1 MHz)2.35
Dissipation Factor (1 MHz)3×10⁻⁴
Volume Resistivity1×10¹⁶ Ω·cm
Surface Resistivity1×10¹⁵ Ω
Comparative Tracking Index (CTI)600 V

Chemical & Environmental3

Corrosion resistance is excellent (90/100), better than 81% of polymer grades. UV resistance is poor.

Corrosion ResistanceExcellent90/100
UV / Weathering ResistancePoor25/100
Chemical Resistance SummaryExcellent against water, brine, acids, alkalis, alcohols, most salts and aqueous solutions; poor against strong oxidizers (fuming HNO3, halogens); swells in hydrocarbons/chlorinated solvents above ~60 °C; susceptible to environmental stress cracking with surfactants under load.

Sustainability4

Producing a kilogram of HDPE-PCR takes about 25 MJ of energy and emits 0.7 kg of CO₂ — less than 100% of polymer grades. Typical recycled content is 100%.

Embodied Energy (primary production)25 MJ/kg10,748 BTU/lb
Embodied Carbon (primary production)0.7 kg CO₂/kg
Embodied Water90 L/kg10.8 gal/lb
Typical Recycled Content100%

Manufacturability8

HDPE-PCR's machinability is very good (72/100, better than 76% of polymer grades); weldability excellent (95/100); formability very good (70/100).

MachinabilityVery good72/100
WeldabilityExcellent95/100
Formability (cold)Very good70/100
PolishabilityPoor30/100
Mold Shrinkage2%
Melt Flow Rate8 g/10 min
Processing Melt Temperature (typ.)230°C446 °F
Mold Temperature (typ.)40°C104 °F

Values are nominal handbook figures for design screening. Certified mill or lot data ships with every FabDigit order on request.

Other HDPE grades and fills

HDPE is also supplied in 13 other conditions. The full side-by-side table is on the HDPE overview.

Working with HDPE-PCR

Is HDPE easy to machine?

Cuts easily with sharp, high-rake, polished tools and high speed/low feed; use air blast and generous support since heat build-up and low modulus cause gumming, burrs and part distortion.

Can HDPE be welded?

Excellent hot-plate, butt-fusion, electrofusion, hot-gas and extrusion welding (DVS 2207); adhesive bonding requires corona, flame or plasma pre-treatment.

Can HDPE be formed, bent or molded?

Injection, blow, rotational and profile extrusion all standard; melt 200–260 °C, mould 20–60 °C, allow 1.5–3% shrinkage with strong anisotropy and post-mould shrink over 24 h.

What surface finishes work on HDPE?

Cannot be plated or anodized and holds paint poorly; use in-resin colour, laser marking, hot stamping or corona-treated printing, and flame-polish or scrape edges for smooth finishes.

HDPE chemical composition (wt %)

Limits by weight percent from the governing specification, written the way the spec states them — a single maximum for impurities, a range for alloying elements, and the base element as balance. Nominal is the typical mid-range value.

ElementSpec limit (wt %)Nominal
1-butene / 1-hexene comonomershort-chain branching to tune density and ESCR0 – 20.5
antioxidant / process stabilizerhindered phenol + phosphite0.05 – 0.50.2
carbon black2.0–2.5% only in UV-stabilized / pipe grades0 – 2.50
ethylene (polyethylene chain)linear homopolymer backbone≥ 97 (balance)

HDPE-PCR — frequently asked

What is HDPE-PCR used for?

HDPE-PCR is typically used for cutting boards and food-contact surfaces, PE100 pressure pipe and fittings, chemical and water storage tanks, blow-moulded bottles and jerricans, playground equipment panels and conveyor wear strips and guides. In short: chemical resistant; budget.

What is the yield strength of HDPE-PCR?

HDPE-PCR has a typical yield strength of 22 MPa (3.19 ksi) and a tensile strength of 23 MPa (3.34 ksi) — weaker than 83% of polymer grades. Strength varies by condition: see the 14 listed tempers.

Is HDPE-PCR easy to machine?

Yes — machinability is rated very good (72/100, better than 76% of polymer grades). Cuts easily with sharp, high-rake, polished tools and high speed/low feed; use air blast and generous support since heat build-up and low modulus cause gumming, burrs and part distortion.

Can HDPE-PCR be welded?

Yes — weldability is rated excellent (95/100). Excellent hot-plate, butt-fusion, electrofusion, hot-gas and extrusion welding (DVS 2207); adhesive bonding requires corona, flame or plasma pre-treatment.

What surface finishes work on HDPE-PCR?

Cannot be plated or anodized and holds paint poorly; use in-resin colour, laser marking, hot stamping or corona-treated printing, and flame-polish or scrape edges for smooth finishes.

Can HDPE-PCR be formed, bent or molded?

Injection, blow, rotational and profile extrusion all standard; melt 200–260 °C, mould 20–60 °C, allow 1.5–3% shrinkage with strong anisotropy and post-mould shrink over 24 h.

What is the maximum service temperature of HDPE-PCR?

HDPE-PCR is rated for continuous use to about 80°C (176 °F), and briefly to 110°C. Strength falls off well before that limit — check the elevated-temperature data for load-bearing parts.

What is the difference between HDPE FDA Compliant and HDPE-GF40?

FDA Compliant is the default condition — choose for cutting boards, food processing parts, potable water and pharma contact; additive package limited to FDA 21 CFR 177.1520 / EU 10-2011 listed stabilizers. GF40: highly reinforced HDPE with 40% coupled short glass fiber — maximum stiffness, strength and dimensional stability in the PE family, used for structural and under-hood-type mouldings. Yield strength is 26 MPa in FDA Compliant versus 78 MPa in GF40.

Can FabDigit make parts in HDPE-PCR?

Yes — HDPE-PCR is available for CNC machining, sheet metal and injection molding with instant online pricing. Upload a STEP file to get a price and a DFM check.

Sources

  1. ASTM D4976 — Standard Specification for Polyethylene Plastics Molding and Extrusion MaterialsASTM International (2020)
  2. ISO 1872-1/-2 — Plastics: Polyethylene (PE) moulding and extrusion materialsISO (2015)
  3. Engineered Materials Handbook Vol. 2 — Engineering PlasticsASM International (1988)
  4. CAMPUS Plastics — HDPE datasheets (ISO 10350 property set)CAMPUS Consortium (2024)
  5. Hostalen / Lupolen HDPE grade datasheetsLyondellBasell (2023)
  6. Sclair HDPE resin datasheetsNOVA Chemicals (2023)

Property data is compiled from published supplier and standards handbooks and normalised for comparison. Nothing on this page is a certification — request mill certs, CoC or material test reports with your order.