FabDigit

Ash · finish state

Ash-GRN

Properties of the GRN condition, compared with the other Ash tempers.

Pick for steam bending, turning blanks and riven handle stock that will be dried after shaping.

Standard cost $$

What is Ash-GRN?

Ash-GRN is Ash supplied in the GRN condition — pick for steam bending, turning blanks and riven handle stock that will be dried after shaping. Ash-GRN has a tensile strength of 75 MPa (10.9 ksi), stronger than 70% of natural material grades. Elongation at break is 1% and the elastic modulus is 9.9 GPa (1.44 Msi). Ash-GRN has a density of 0.87 g/cm³ (0.0314 lb/in³), heavier than 70% of natural material grades. KD12 is the default condition FabDigit quotes; GRN is available on request or by drawing note.

Advantages

  • Conducts heat well — 0.28 W/m·K (0.162 BTU/hr·ft·°F), better than 81% of natural material grades

Limitations

  • Needs corrosion protection — 20/100, worse than 98% of natural material grades
  • Limited service temperature — 60°C (140 °F), worse than 94% of natural material grades
  • Difficult to machine — 55/100, worse than 91% of natural material grades

Ash-GRN properties

Typical room-temperature values for Ash-GRN — 11 properties are specific to this condition; the rest are grade-level values shared by every Ash temper. Each bar shows where the value sits among the natural material grades in FabDigit's library — further right is higher.

Physical2

Ash-GRN has a density of 0.87 g/cm³ (0.0314 lb/in³), heavier than 70% of natural material grades.

Density0.87 g/cm³0.03 lb/in³
Porosity55%

Mechanical9

Ash-GRN has a tensile strength of 75 MPa (10.9 ksi), stronger than 70% of natural material grades. Elongation at break is 1% and the elastic modulus is 9.9 GPa (1.44 Msi).

Elastic (Young's) Modulus9.9 GPa1.4 Msi
Shear Modulus0.95 GPa0.14 Msi
Poisson's Ratio0.37
Tensile Strength (Ultimate)75 MPa10.9 ksi
Elongation at Break1%
Compressive Strength27 MPa3.9 ksi
Flexural Strength66 MPa9.6 ksi
Shear Strength9 MPa1.3 ksi
Fracture Toughness (K_IC)0.5 MPa·√m0.46 ksi·√in

Thermal5

Ash-GRN is rated for continuous service to 60°C (140 °F). It conducts heat at 0.28 W/m·K (0.162 BTU/hr·ft·°F), better than 81% of natural material grades. Thermal expansion is 30 µm/m·K (16.7 µin/in·°F).

Thermal Conductivity0.28 W/m·K0.16 BTU/hr·ft·°F
Specific Heat Capacity1,700 J/kg·K0.41 BTU/lb·°F
Thermal Expansion (CTE, 20–100 °C)30 µm/m·K16.7 µin/in·°F
Max Service Temperature (continuous)60°C140 °F
Min Service Temperature-60°C-76 °F

Electrical2

Ash-GRN is an electrical insulator with a dielectric strength of 3 kV/mm (76.2 V/mil) and a resistivity of 100 Ω·m.

Electrical Resistivity100 Ω·m3.94×10⁹ µΩ·in
Dielectric Strength3 kV/mm76.2 V/mil

Chemical & Environmental1

Corrosion resistance is poor (20/100), worse than 98% of natural material grades.

Corrosion ResistancePoor20/100

Sustainability4

Producing a kilogram of Ash-GRN takes about 11 MJ of energy and emits 0.5 kg of CO₂ — more than 56% of natural material grades. Typical recycled content is 5%.

Embodied Energy (primary production)11 MJ/kg4,729 BTU/lb
Embodied Carbon (primary production)0.5 kg CO₂/kg
Embodied Water650 L/kg77.9 gal/lb
Typical Recycled Content5%

Manufacturability2

Ash-GRN's machinability is good (55/100, worse than 91% of natural material grades).

MachinabilityGood55/100
PolishabilityGood55/100

Values are nominal handbook figures for design screening. Certified mill or lot data ships with every FabDigit order on request.

Other Ash tempers and conditions

Ash is also supplied in 3 other conditions. The full side-by-side table is on the Ash overview.

Working with Ash-GRN

Is Ash easy to machine?

Saws, planes and turns cleanly with carbide tooling; moderate tool blunting and a tendency to tear-out at interlocked grain, so use sharp knives and light finishing cuts.

Can Ash be welded?

Not weldable — joined by PVAc/PU/epoxy adhesives (glues well) or mechanical fasteners; pre-drill near ends to avoid splitting.

Can Ash be formed, bent or molded?

One of the best steam-bending hardwoods: steam green or air-dried stock ~1 h per 25 mm and bend over a strap to tight radii.

What surface finishes work on Ash?

Coarse open pores need grain filler for a mirror finish; stains, oils and waterborne lacquers take evenly, and exterior use requires preservative or thermal modification plus UV-stable coating.

Ash chemical composition (wt %)

Limits by weight percent from the governing specification, written the way the spec states them — a single maximum for impurities, a range for alloying elements, and the base element as balance. Nominal is the typical mid-range value.

ElementSpec limit (wt %)Nominal
celluloseoven-dry basis40 – 4744
hemicellulosexylan-rich, typical of hardwoods22 – 3026
ligninsyringyl/guaiacyl type21 – 2825
extractivestannins, fats, sugars; higher in heartwood2 – 64
mineral ashCa, K dominated0.2 – 10.6
moisture (as supplied, KD)added on top of oven-dry substance8 – 1412

Ash-GRN — frequently asked

What is Ash-GRN used for?

Ash-GRN is typically used for tool handles, baseball bats, hockey sticks, furniture and interior trim. In short: highest shock resistance here; excellent steam-bending hardwood; open-pore surface needs filler.

What is the tensile strength of Ash-GRN?

Ash-GRN has a typical tensile strength of 75 MPa (10.9 ksi) — stronger than 70% of natural material grades. Strength varies by condition: see the 4 listed tempers.

Is Ash-GRN easy to machine?

Reasonably — machinability is rated good (55/100, worse than 91% of natural material grades). Saws, planes and turns cleanly with carbide tooling; moderate tool blunting and a tendency to tear-out at interlocked grain, so use sharp knives and light finishing cuts.

Can Ash-GRN be welded?

Not weldable — joined by PVAc/PU/epoxy adhesives (glues well) or mechanical fasteners; pre-drill near ends to avoid splitting.

What surface finishes work on Ash-GRN?

Coarse open pores need grain filler for a mirror finish; stains, oils and waterborne lacquers take evenly, and exterior use requires preservative or thermal modification plus UV-stable coating.

Can Ash-GRN be formed, bent or molded?

One of the best steam-bending hardwoods: steam green or air-dried stock ~1 h per 25 mm and bend over a strap to tight radii.

What is the maximum service temperature of Ash-GRN?

Ash-GRN is rated for continuous use to about 60°C (140 °F). Strength falls off well before that limit — check the elevated-temperature data for load-bearing parts.

Sources

  1. Wood Handbook — Wood as an Engineering Material (FPL-GTR-190), mechanical properties of white/green ashUSDA Forest Products Laboratory (2021)
  2. EN 13556 — Round and sawn timber: nomenclature of timbers used in Europe (FRAX)CEN (2003)
  3. EN 350 — Durability of wood and wood-based products, natural durability classesCEN (2016)
  4. The Wood Database — Fraxinus excelsior / Fraxinus americana species datawood-database (2023)
  5. Thermally modified ash cladding technical data (Thermory/ThermoWood class D)International ThermoWood Association (2022)

Property data is compiled from published supplier and standards handbooks and normalised for comparison. Nothing on this page is a certification — request mill certs, CoC or material test reports with your order.